Pipe fittings are the general names of parts and components that play the role of connection, control, direction change, diversion, sealing and support in the pipeline system. Steel fittings are pressure fittings. According to the different processing technology, it is divided into four categories, namely, butt welding pipe fittings (divided into weld and no weld), socket welding and threaded pipe fittings, flange pipe fittings.
According to the application:
1. pipe fittings for connecting pipes are: flanges, live joints, pipe hoops, clamps, clamps, throat hoops, etc.
2. changing the direction of the pipe: bends, bends.
3. pipe fittings changing pipe diameter: variable diameter (different diameter pipe), different diameter elbow, branch pipe table, reinforcing pipe.
4. pipe fittings with additional piping branches: three links, four links.
5. pipe fittings for pipe sealing: gasket, raw material belt, thread, flange blind plate, pipe plug, blind plate, head, welding plug.
6. pipe fittings for pipe fixing: clasp, hook, ring, bracket, bracket, pipe clamp, etc.
According to the connection :1, welded pipe fittings 2, threaded pipe fittings 3, clamping pipe fittings 4, clamping pipe fittings 5, socket pipe fittings 6, rubber ring connection pipe fittings
According to the material divided into 1, cast steel pipe fittings 2, forged steel pipe fittings 3, alloy pipe fittings 4, stainless steel pipe fittings.
Pipe fittings are widely used in municipal, petrochemical, west-to-east gas transmission, ships and nuclear power.
Raw melting material - aluminum scraps, cans, engine waste etc.
Output capacity - 5-30 tons/h, customized
Automation - Full automatic/ half automatic (based on output requirement and investment budget
Ingot type - ADC12 (7.5kg/ 10kg / customized)
1. After cleaning the oil and grease of waste aluminum, manually put it into the furnace with a forklift;
2. Ignition for melting furnace .Heat up to 680C, and input appropriate proportion of alloy elements. Heat up to 800C, melt and stir evenly, then fetch samples to the spectrometer for testing.
Every lot of production need to do testing .
3. Put A tool that attracts iron into the furnace by forklift, to suck away the iron in the aluminum water.
4. Put the slag agent into Alu liquid to remove the slag. After slag removed , put the slags into Aluminum ash separation machine , and let the aluminum water and ash separate. The proportion of slag agent and aluminum liquid is 1:500
5.Open the drain valve and the aluminum water flows automatically to the ingot production line After the ingot casting is completed, the ingot stacking robot will stack the ingots, which means the production is completed.