Co-based amorphous core in plastic container
1. high permeability
2.Thickness (1820 mkm)
3. Annealing in transverse field, permeability more than 100000, very low loss, flat hysteresis loop
4. Common-mode filter chokes, current transformers, including for precise electronic electricity meters, protective cutout, High Frequency power transformers in SMPS, audio transformers, etc.
5.D from 4-32mm
Ribbon wound magnetic core is placed into hard protective container of glass-polyamide and mechanically fixed with silicone sealant.
Co-based amorphous ribbon wound magnetic core is placed into hard protective container of glass-polyamide and mechanically fixed with silicone sealant.Size veries:outer D =4-32mm.The container has rounded edges and is designed for direct winding of a thick wire. The container provides reliable mechanical protection and preservation of amorphous material's properties. All materials comply with UL94V-1 / 0.
1. High permeability
2.Thickness (1820 mkm)
3. Annealing in transverse field, permeability more than 100000, very low loss, flat hysteresis loop
4. KEY FEATURES OF THE AMORPHOUS MATERIAL:
Induction amplitude, Bm (25C) 0.59 T
Induction amplitude, Bm (90C) 0.50 T
Curie temperature, Tc 220C
Operating temperature range -60C ... 100C
Magnetostriction less than 0.110^-6
Typical permeability (10 kHz) - 120 000
Typical permeability (100 kHz) - 35 000